Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 152 J/g | 65.4 BTU/lb | DSC |
Total 3802 B HDPE, cable, sheet, pipe, injection molding FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene.. |