Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 34.7 J/g | 14.9 BTU/lb | |
Indium Corp. Indalloy 39 Bismuth Solder Alloy Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation |