Polymer Property : Minimum Service Temperature, Air = 93.3 °C
Polymer Property :
Minimum Service Temperature, Air =
93.3 °C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Minimum Service Temperature, Air
93.3
°C
200
°F
Monmouth Rubber & Plastics Durafoamâ„¢ IVN 41 NEO/PVC/NBR
Information provided by Monmouth Rubber & Plastics Corp.