Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 899 °C | 1650 °F | Lower limit of working range |
Heatbath/Park Petroleum Pitch Coke Neutral Pack A granular material widely used as a packing medium for high carbon chromium tool steels to prevent undesirable carburization or decarburization. Used similarly to crushed coke but offers more unifo.. |