Polymer Property : Minimum Service Temperature, Air = 760 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 760 °C
1400 °F
Lower limit of working range
Heatbath/Park Carbon Cover
A specially selected graphite which can be used as a floating cover on molten neutral salt baths or as additional cover for carburizing salts. Park Carbon supplements the cover material incorporated..
Minimum Service Temperature, Air 760 °C
1400 °F
Lower limit of working range
Heatbath/Park Carbon Cover C
A special blend of graphites suited for cover on neutral salts especially for use with Nu-SalInformation provided by Heatbath Corporation - Park Metallurgical.
Minimum Service Temperature, Air 760 °C
1400 °F
Lower limit of working range
Heatbath/Park No-Carb Stop-Off/Protective Coating for Steel
Water-base paint containing copper used to prevent carburization or decarburization of steel during heating for hardening, carburizing, annealing, normalizing, forging or rollingInformation provided..
Minimum Service Temperature, Air 760 °C
1400 °F
Lower limit of working range
Heatbath/Park No-Carb 1397 Stop-Off/Protective Coating for Steel
A new, water-washable, stop-off compound for gas, vacuum or pack carburizing. Effective stop-off for case depths to .250" at temperatures as high as 1800°FInformation provided by Heatbath Corpor..
Minimum Service Temperature, Air 760 °C
1400 °F
Lower limit of working range
Heatbath/Park No-Carb Special Stop-Off/Protective Coating for Steel
Similar to No-Carb, but with a thicker, heavy duty formulation for special applications.Information provided by Heatbath Corporation - Park Metallurgical.