Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 704 °C | 1300 °F | Lower limit of working range |
Heatbath/Park Nu-Sal High Speed Hardening Salt This barium-free salt is the most economical and most commonly used neutral salt for heat treating performed within its working range. It is non-hygroscopic and relatively non-corrosive to metal an.. |
|||
Minimum Service Temperature, Air | 704 °C | 1300 °F | Lower limit of working range |
Heatbath/Park Nu-Sal Neutral Salt This barium-free salt is the most economical and most commonly used neutral salt for heat treating performed within its working range. It is non-hygroscopic and relatively non-corrosive to metal an.. |
|||
Minimum Service Temperature, Air | 704 °C | 1300 °F | Lower limit of working range |
Heatbath/Park Nu-Sal Steel Brazing Neutral Salt The most economical salt for brazing performed within its working range. Silver and brass brazing are commonly done in Nu-Sal. It is non-hygroscopic and relatively non-corrosive to metal and fixture.. |
|||
Minimum Service Temperature, Air | 704 °C | 1300 °F | Lower limit of working range |
Heatbath/Park Sta-Hard 17 High Speed Hardening Salt A neutral salt for hardening, annealing, normalizing, or preheating high speed tools. It is non-decarburizing, making it suitable for heating alloy tool steels which require high hardening temperatu.. |
|||
Minimum Service Temperature, Air | 704 °C | 1300 °F | Lower limit of working range |
Heatbath/Park Sta-Hard 17 Neutral Salt A neutral salt for hardening, annealing, normalizing, or preheating high speed tools. It is non-decarburizing, making it suitable for heating alloy tool steels which require high hardening temperatu.. |