Thermal Properties Metric English Comments
Minimum Service Temperature, Air 332 °C
630 °F
Lower limit of working range
Heatbath/Park AL-3 High Speed Hardening Salt
A low-cost granular mixture of nitrates formulated for tempering steels where the lower melting point and wider working range of AL-2 are not needed. Like AL-2, AL-3 is a highly fluid bath that offe..