Thermal Properties Metric English Comments
Minimum Service Temperature, Air -14.7 °C
5.54 °F
Gehman torsion test, T10
Daikin DAI-EL G-671 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 67% Fluorine Content
Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Excellent low-temperature sealing ..