Thermal Properties Metric English Comments
Minimum Service Temperature, Air -65.0 - 2.22 °C
-85.0 - 36.0 °F
Average value: -20.0 °C Grade Count:299
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..