Polymer Property : Minimum Service Temperature, Air = 260 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 260 °C
500 °F
Lower limit of working range
Heatbath/Park Draw Black Cleaning Salt
A salt designed for rapid, thorough and economical cleaning of dies, molds and miscellaneous hardware used in the fabrication of plastics. Also, effective in removing paints, organic binders, oils a..