Polymer Property : Minimum Service Temperature, Air = 18.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 18.0 °C
64.4 °F
Brush
ChevronTexaco Compound L Rust Proof
Texaco Rust Proof Compounds deliver value through:Excellent long-term rust protection — Petrolatum and special additive system form a nonhardening, self sealing film to protect surfaces against the..