Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 38.0 - 54.0 °C | 100 - 129 °F | Spray |
ChevronTexaco Compound L Rust Proof Texaco Rust Proof Compounds deliver value through:Excellent long-term rust protection — Petrolatum and special additive system form a nonhardening, self sealing film to protect surfaces against the.. |