Thermal Properties Metric English Comments
Minimum Service Temperature, Air -7.61 °C
18.3 °F
Arlon 680-R3839R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate
Design/Construction:Side 1: Cured Silicone Coating Substrate: Silica-basedSide 2: Cured Silicone Coating Rubber Application Advantages:Extremely low thermal conductivityThermally stableBondable to s..
Minimum Service Temperature, Air -7.61 °C
18.3 °F
Arlon 680-R3844R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate
Design/Construction:Side 1: Cured Silicone Coating Substrate: Silica-basedSide 2: Cured Silicone Coating Rubber Application Advantages:Extremely low thermal conductivityThermally stableBondable to s..