Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -59.0 °C
-74.2 °F
Cured
Parker Chomerics Tecknit CON/RTV-I One Part: Silver-Filled Silicone RTV
Description: TECKNIT CON/RTV-I system is a pure silver loaded, one component RTV silicone adhesive sealant. It is ready to use without mixing and cures quickly at room temperature on exposure to moi..
Minimum Service Temperature, Air -59.0 °C
-74.2 °F
Dow Corning 1890 PROTECTIVE COATING
Silicone RTV in solvent dispersionInformation provided by Dow Corning