Polymer Property : Minimum Service Temperature, Air = -55.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -48.3 °C
-55.0 °F
ConocoPhillips Syncon® HP Synthetic Grease NLGI No. 1
Description: Conoco Syncon HP Synthetic Grease is a high-quality, synthetic polyalphaolefin (PAO) lithium grease developed to provide exceptional protection and corrosion resistance for bearings and..