Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -42.8 °C | -45.0 °F | Approx. Cold test |
Lubriplate SYN SYN-1602 PAO-Based Multi-Purpose Grease Manufactured with 100% PAO base fluids and thickened with lithium complex for superior oxidation stability, better wear protection, and significantly better operating temperature ranges. Fortified w.. |
|||
Minimum Service Temperature, Air | -42.8 °C | -45.0 °F | |
Master Bond MasterSil 708FR One Part, Flame Resistant Silicone Description: MasterSil 708FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V.1 for thicknesses of .. |