Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -226 °C | -375 °F | Embrittlement Temp |
TriStar Ultracomp UC-200 Composite Bearing Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m.. |
|||
Minimum Service Temperature, Air | -226 °C | -375 °F | Embrittlement Temp |
TriStar Ultracomp UC-300 Composite Bearing Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family.. |