Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -65.0 - -27.0 °C | -85.0 - -16.6 °F | Average value: -41.9 °C Grade Count:17 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |