Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -32.2 °C | -26.0 °F | Lowest Temp Tested for Bullet Resistance |
Spartech Polycast MP 1.25 (UL 752 Level 1) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Minimum Service Temperature, Air | -32.2 °C | -26.0 °F | Lowest Temp Tested for Bullet Resistance |
Spartech Polycast SAR HP 1.25 (UL 752 Level 3) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Minimum Service Temperature, Air | -32.2 °C | -26.0 °F | Lowest Temp Tested for Bullet Resistance |
Spartech Polycast SP 1.25 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |