Thermal Properties Metric English Comments
Minimum Service Temperature, Air -18.9 °C
-2.00 °F
Retraction Temperature, TR10; ASTM D1329
Seals Eastern 5717 Fluorocarbon-Elastomer
FKM. General service.Information provided by Seals Eastern, Inc.