Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -121 - 45.0 °C | -185 - 113 °F | Average value: -56.9 °C Grade Count:128 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Minimum Service Temperature, Air | -121 °C | -185 °F | |
Master Bond Mastersil 415 One Component Room Temperature Curing, Transparent Silicon Master Bond MasterSil 415 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing and protective coatings featuring high transparency. It has a paste consi.. |