Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 85.0 - 96.0 °C | 185 - 205 °F | Average value: 90.9 °C Grade Count:16 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |