Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 96.0 °C | 205 °F | ExxonMobil Method |
ExxonMobil LD 145.PX Packaging Resin
(discontinued **) LD 145.PX resin is a homopolymer cast film resin offering good clarity and toughness. Applications include Bread bags and other Food Packaging.Information provided by ExxonMobil Chemical |
|||
Crystallization Temperature | 96.0 °C | 205 °F | ExxonMobil Method |
ExxonMobil LD 316.19 High Clarity, High Impact Film Resin LD 316.19 has improved impact strength and heat sealability versus homopolymer clarity film resins. Applications include frozen and other food packaging, as well as profile extrusion.Information pr.. |