Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 29.0 °C | 84.2 °F | ExxonMobil Method |
ExxonMobil Exact™ 9061 Ethylene-based Plastomer Resin Product Description: Exact 9061 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |