Polymer Property : Crystallization Temperature = 81.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 81.0 °C
178 °F
Dow Method
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA)
AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional ..