Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 80.0 °C | 176 °F | Dow Method |
Dow AMPLIFY™ EA 102 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 102 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |