Polymer Property : Crystallization Temperature = 75.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 75.0 °C
167 °F
Reltek BONDiT™ HM-502 Coating, Sealant, Adhesive System
A protective coat for most metal, glass, and ceramic materials for use against corrosion and other chemical attacks. Useful against fungi growth. Bondit HM-502 is a thermoplastic emulsion system.Inf..
Crystallization Temperature 75.0 °C
167 °F
Reltek BONDiT™ HM-505 Coating, Sealant, Adhesive System
Information provided by Reltek LLC