Thermal Properties Metric English Comments
Crystallization Temperature 56.0 °C
133 °F
ExxonMobil Method
ExxonMobil EXACT™ 4056 Plastomer for Film Blends and Blown Film Applications
Product Description: Exact 4056 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin can be used in blends with polyolefins to improve..