Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 252 °C | 486 °F | ISO 3146 |
ExxonMobil PP7054L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with medium flow. It is suitable for molding applications like consumer products, closures, containers, toys and rigid packaging applications.. |