Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 310 - 315 °C | 590 - 599 °F | |
Solvay Specialty Polymers Polymist® F-5 PTFE Powder Lubricant
(discontinued **) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |
|||
Crystallization Temperature | 310 - 315 °C | 590 - 599 °F | |
Solvay Specialty Polymers Polymist® F-5A PTFE Powder Lubricant
(Unverified Data**) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |