Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | >= 155 °C | >= 311 °F | Grade H1 |
Kazanorgsintez Bisphenol A, Diphenylpropane Production Method: Bisphenol A is obtained by condensation of phenol and acetone in presence of catalyst. Application: Intended for production of polycarbonates, polysulfones, epoxy resins, lacquers.. |