Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 275 - 285 °C
527 - 545 °F
Peak; ASTM D3418
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance..
Crystallization Temperature 275 - 285 °C
527 - 545 °F
Peak; ASTM D3418
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Crystallization Temperature 275 - 285 °C
527 - 545 °F
Peak, DSC
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, ..
Crystallization Temperature 275 - 285 °C
527 - 545 °F
Peak, DSC
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..