Polymer Property : Crystallization Temperature = 264 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 129 °C
264 °F
Melting; DSC
LG Chemical LUTENE-H XL1800 HDPE
Description: LUTENE-H XL 1800 is a optimum materials for under-floor heating and drinking water pipe by RAM type extrusion. It is excellent product with long-term internal pressure creep property an..