Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 237 °C
459 °F
ISO 3164
ExxonMobil PP1014H1 Polypropylene Homopolymer
Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE..
Crystallization Temperature 237 °C
459 °F
ISO 3146
ExxonMobil PP1064L1 Polypropylene Homopolymer
Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other ..
Crystallization Temperature 237 °C
459 °F
ISO 3146
ExxonMobil PP1364E2 Polypropylene Homopolymer
Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer produc..