Polymer Property : Crystallization Temperature = 192 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 89.0 - 93.0 °C
192 - 199 °F
Peak; ASTM D3418
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit..
Crystallization Temperature 89.0 °C
192 °F
ExxonMobil Method
ExxonMobil LD 306.38 High Clarity, High Impact Film Resin
LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical
Crystallization Temperature 89.0 °C
192 °F
ExxonMobil Method
ExxonMobil LD 306.57 High Clarity, High Impact Film Resin
LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical
Crystallization Temperature 89.0 °C
192 °F
ExxonMobil Method
ExxonMobil LD 306.75 High Clarity, High Impact Film Resin
LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical
Crystallization Temperature 89.0 °C
192 °F
ExxonMobil Method
ExxonMobil LD 307.76 Clear, High Impact Film Resin
LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical
Crystallization Temperature 89.0 - 93.0 °C
192 - 199 °F
Peak, DSC; ASTM D3418
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers.