Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | >= 156.7 °C | >= 314.1 °F | Grade HF |
Kazanorgsintez Bisphenol A, Diphenylpropane Production Method: Bisphenol A is obtained by condensation of phenol and acetone in presence of catalyst. Application: Intended for production of polycarbonates, polysulfones, epoxy resins, lacquers.. |