Thermal Properties Metric English Comments
Crystallization Temperature 58.0 °C
136 °F
DSC, 10°C/min (peak); DuPont Test
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer
Description: ENR 7256.00 is a unique broader molecular weight distribution ethylene-butene copolymer with higher branching levels that offers excellent clarity, processing and performance in foams a..