Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 134 - 144 °C | 273 - 291 °F | Peak, DSC; ASTM D3418 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Crystallization Temperature | 134 - 144 °C | 273 - 291 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF) Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope.. |
|||
Crystallization Temperature | 134 - 144 °C | 273 - 291 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
Crystallization Temperature | 134 °C | 273 °F | Melting; DSC |
LG Chemical LUTENE-H ME8000 HDPE Description: LUTENE-H ME8000 is mainly intended for injection molding of containers. It has good mechanical properties and high productivity.Applications: Silicone cartridge, containers, complicated.. |