Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 35.0 - 50.0 °C | 95.0 - 122 °F | |
Addcomp PRIEX® 25050 Maleic Anhydride Grafted PP random copolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Crystallization Temperature | 35.0 - 50.0 °C | 95.0 - 122 °F | |
Addcomp PRIEX® 25095 Maleic Anhydride Grafted PP random copolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |