Polymer Property : Crystallization Temperature = 118 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 118 °C
244 °F
Dow Method (DSC)
Dow DMDA-8907 NT 7 High Density Polyethylene Resin
DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information..
Crystallization Temperature 118 °C
244 °F
Dow Method (DSC)
Dow DMDB-7950 NT 7 High Density Polyethylene Resin
DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo..
Crystallization Temperature 118 °C
244 °F
Dow Method (DSC)
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE)
Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6200 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol..
Crystallization Temperature 118 °C
244 °F
Dow Method (DSC)
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE)
Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to..
Crystallization Temperature 118 °C
244 °F
Dow Method (DSC)
Dow UNIVAL™ DMDA-6320 NT 7 High Density Polyethylene Resin (HDPE)
Low swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6320 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package household..
Crystallization Temperature 118 °C
244 °F
Dow Method (DSC)
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE)
Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to..