Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 117 °C | 243 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ S10 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:Excellent stiffnessFair impact resistanceFair processingTypical Applications: High-load/High performance products, such as .. |
|||
Crystallization Temperature | 117 °C | 243 °F | Dow Method (DSC) |
Dow DMDA-8920 NT 7 High Density Polyethylene Resin DOW DMDA-8920 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |
|||
Crystallization Temperature | 117 °C | 243 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE) Good extrudability/processability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This produ.. |
|||
Crystallization Temperature | 117 °C | 243 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDC-6145 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6145 NT 7 provides good parison stability, which contribu.. |