Polymer Property : Crystallization Temperature = 116.1 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 116.1 °C
241.0 °F
ASTM D3418
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade
ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces..