Polymer Property : Crystallization Temperature = 115.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 115.9 °C
240.6 °F
ASTM D3418
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade
ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case..