Polymer Property : Vicat Softening Point = 99.4 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 99.4 °C
211 °F
ASTM D-1525
Plaskolite Optix® CP - 1000 IG High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Vicat Softening Point 99.4 °C
211 °F
ASTM D-1525
Plaskolite West Optix® CP - 1000 IG High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Vicat Softening Point 99.4 °C
211 °F
120°C/hr, 1 kg; ASTM D1525-B
Americas Styrenics STYRON™ 666LR General Purpose Polystyrene Resin  (discontinued **)
STYRON™ 666LR is a medium flow general purpose polystyrene specifically designed to blend with styrene butadiene styrene block copolymers for packaging applications requiring high clarity, improved..
Vicat Softening Point 99.4 °C
211 °F
ASTM D1525
ExxonMobil LL 6202 Injection Molding Resin  (discontinued **)
LL 6202 is a narrow molecular weight butene copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that require outstanding tear..
Vicat Softening Point 99.4 °C
211 °F
Rate A (50°C/h), Loading 1 (10 N); ASTM D1525
Entec Hyrene® PS-HI 3/3 High Impact Polystyrene
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec