Polymer Property : Vicat Softening Point = 97.5 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 97.5 °C

@Load 1.00 kg,
Thickness 3.17 mm
208 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Diamond Polymers SBS 2160 Clear Styrene Butadiene Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.