Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 91.7 °C | 197 °F | ASTM D1525 |
ExxonMobil LL 6201 Injection Molding Resin
(discontinued **) LL 6201 is a narrow molecular weight butene copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications .. |
|||
Vicat Softening Point | 91.7 °C | 197 °F | ASTM D1525 |
ExxonMobil LD 103.MP Industrial Film Resin
(discontinued **) LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati.. |
|||
Vicat Softening Point | 91.7 °C | 197 °F | ASTM D1525 |
ExxonMobil LD 146.NH Cast Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 91.7 °C | 197 °F | ASTM D1525 |
ExxonMobil LD 146.NH Packaging Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 91.7 °C | 197 °F | ASTM D1525 |
ExxonMobil LD 641.LN Molding, Extrusion and Compounding Resin
(discontinued **) LD 641.LN is a low density homopolymer specifically designed for high performance blow molding applications. This resin is suitable for applications requiring high melt strength, flexibility, good .. |
|||
Vicat Softening Point | 91.7 °C | 197 °F | ASTM D1525 |
Total PSI 830 Polystyrene Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The m.. |