Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 26.7 °C | 80.0 °F | ASTM D1525 |
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |