Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 66.0 - 68.0 °C @Load 5.00 kg |
151 - 154 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds ART 0665/S Rigid PVC, Atoxic for General Purpose Injection moulding and blow moulding bottles |