Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 57.8 °C | 136 °F | ASTM D1525 |
ExxonMobil Escorene® LD 722.MV Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 722.MV is a high vinyl acetate copolymer resin for specialty extrusion and compounding application. Articles made from LD 722.MV are soft and have excellent low temperature toughne.. |