Vicat Softening Point | 52.0 - 54.0 °C @Load 5.00 kg |
126 - 129 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RST 0447/1 Rigid PVC, Extrusion Lead Free Extrusion transparent films |